Thermal Properties | Metric | English | Comments |
---|---|---|---|
Clash Berg Stiffness Temperature | -39.0 °C | -38.2 °F | |
Dow Pellethane® 2102-90AE Polyurethane Elastomer, Polyester Polycaprolactone Based
(discontinued **) PELLETHANE® 2102-90AE elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with good damping capacity and good hydrolytic sta.. |
|||
Clash Berg Stiffness Temperature | -39.0 °C | -38.2 °F | |
Dow Pellethane® 2102-90AR Polyurethane Elastomer, Polyester Polycaprolactone Based
(discontinued **) PELLETHANE® 2102-90AR elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with enhanced mold release, low compression set, a.. |