Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature, Tg | 525 °C | 977 °F | ISO 7884-8 |
Schott DURAN® Borosilicate Glass Borosilicate glass 3.3 acc. To ISO 3585, chemically and thermally highly resistant, general-purpose glass for apparatus for the chemical industry, for pipelines, and glasswareInformation provided by.. |
|||
Transformation Temperature, Tg | 525 °C | 977 °F | ISO 7884-8 |
Schott DURATAN® Borosilicate Glass Prestressed borosilicate glass 3.3, chemically and thermally highly resistant, Flameproof lighting The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below .. |
|||
Transformation Temperature, Tg | 525 °C | 977 °F | ISO 7884-8 |
Schott Glass 8347 Borosilicate Glass Borosilicate glass 3.3 acc. To ISO 3585, chemically and thermally highly resistant, highly UV-transmitting The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium i.. |
|||
Transformation Temperature, Tg | 525 °C | 977 °F | ISO 7884-8 |
Schott Glass 8487 Borosilicate Glass Borosilicate glass for sealing to tungsten Backlights, flash lamps, lamp bulbs, exhaust and flare bulbs The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is .. |
|||
Transformation Temperature, Tg | 525 °C | 977 °F | ISO 7884-8 |
Schott Glass 8687 Borosilicate Glass Borosilicate glass for sealing to tungsten, defined UV absorption, stabilized against solarization Backlights The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromi.. |
|||
Transformation Temperature, Tg | 525 °C | 977 °F | ISO 7884-8 |
Schott KIMAX® Borosilicate Glass Laboratory Glass Drainline from Borosilicate glass 3.3. Chemically and thermally highly resistant.The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below 10.. |
|||
Transformation Temperature, Tg | 525 °C | 977 °F | |
Schott AR-GLAS® Soda Lime Silicate Glass Soda lime silicate glass, high dielectric constant, glass to metal seal, pharmaceutical primary packaging, general technical applicationInformation provided by SCHOTT AG. |
|||
Transformation Temperature, Tg | 525 °C | 977 °F | |
Schott BORO-8330â„¢ Borosilicate Glass Borosilicate glass 3.3 acc. ISO 3585, chemically highly resistant, highly resistant to thermal shock, special applications in the pharmaceutical industryInformation provided by SCHOTT AG. |
|||
Transformation Temperature, Tg | 525 °C | 977 °F | ISO 7884-8 |
Schott CONTURAX® Borosilicate Glass Borosilicate glass tubing and rod, varying types of inner and outer shapes Lighting, giftware, and decoration The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromi.. |