Thermal Properties Metric English Comments
Transformation Temperature, Tg 500 °C
932 °F
ISO 7884-8
Schott Glass 8688 Borosilicate Glass
Borosilicate glass, highly UV-blocked, stabilized against solarization, sealing glass to Tungsten Backlights The heavy metal content of the elements lead, cadmium, mercury, and hexavalent chromium..
Transformation Temperature, Tg 500 °C
932 °F
Schott LAFN7 Glass
Information Provided by SCHOTT North America, Inc.