Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature, Tg | 418 °C | 784 °F | |
Mo-Sci Corporation GAI-40-I Green A Intruder Filter Glass Applications: Lead-free NVIS Green A Intruder filter glass for incandescent light sources.Information provided by Mo-Sci Corporation. |