Thermal Properties Metric English Comments
Transformation Temperature, Tg 407 °C
765 °F
Mo-Sci Corporation B-40-I Blue Filter Glass
Applications: Lead-free NVIS blue filter glass for incandescent light source.Information provided by Mo-Sci Corporation.