Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature, Tg | 614 °C | 1140 °F | |
Schott N-LASF43 Glass Information Provided by SCHOTT North America, Inc. |
|||
Transformation Temperature, Tg | 614 °C | 1140 °F | |
Schott N-LAK12 Glass Information Provided by SCHOTT North America, Inc. |