Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature, Tg | 596 °C | 1100 °F | |
Schott OG570 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, GG385, OG590, RG610, RG6.. |