Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature, Tg | 571 °C | 1060 °F | |
Schott RG850 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |
|||
Transformation Temperature, Tg | 571 °C | 1060 °F | |
Schott RG780 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |