Transformation Temperature, Tg 530 °C
986 °F
ISO 7884-8
Schott G018-159 Dental Glass
Remarks: Sr- and Zr-containing, high refractive indexApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provi..
Transformation Temperature, Tg 530 °C
986 °F
Schott P-LASF47 Glass
Suitable for precision moldingInformation Provided by SCHOTT North America, Inc.
Transformation Temperature, Tg 530 °C
986 °F
Schott BOROFLOAT® Borosilicate Float Glass
This is a highly chemically resistant borosilicate glass with a low thermal expansion. BOROFLOAT® replaced TEMPAX®, a drawn flat borosilicate glass for Schott. The high quality resulting fro..