Polymer Property : Transformation Temperature, Tg = 515 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Transformation Temperature, Tg 515 °C
959 °F
ISO 7884-8
Schott Glass 8689 Borosilicate Glass
Borosilicate glass, highly UV-blocked, stabilized against solarization, sealing glass to Tungsten Backlights The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium..