Polymer Property : Transformation Temperature, Tg = 514 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Transformation Temperature, Tg 514 °C
957 °F
ISO 7884-8
Schott Glass 8625 Biocompatible Glass
Biocompatible glass, high IR-absorbing, Transponders (implantable) The heavy metal content of the elements lead, cadmium, mercury, and hexavalent chromium is below 100 ppmInformation provided by S..