Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature, Tg | 470 °C | 878 °F | |
Schott VG14 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
Transformation Temperature, Tg | 470 °C | 878 °F | |
Schott VG6 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
Transformation Temperature, Tg | 470 °C | 878 °F | |
Schott VG9 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |