Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Transformation Temperature, Tg 720 °C
1330 °F
ISO 7884-8
Schott Glass 8252 Alkaline Earth Aluminosilicate Glass
Alkaline earth aluminosilicate glass for high temperature applications in electrical engineering, for sealing to molybdenum, free from alkali Bulb and exhaust tube for halogen lamps for automotive,..
Transformation Temperature, Tg 719 °C
1330 °F
Schott N-LASF31a Glass
Information Provided by SCHOTT North America, Inc.