Polymer Property : Transformation Temperature, Tg = 110 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Transformation Temperature, Tg 110 °C
230 °F
10°C/min; ISO 11357-1/-2
EMS-Grivory Grivory® TR 55 LX PA12/MACMI
Product description: Grilamid TR 55 LX natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 55 LX natural offers outstanding prop..
Transformation Temperature, Tg 110 °C
230 °F
10°C/min; ISO 11357-1/-2
EMS-Grivory Grivory® TR 55 LZ PA12/MACMI
Product description: Grilamid TR grades are transparent thermoplastic polyamides based on aliphatic and cycloaliphatic blocks. Grilamid TR 55 LZ offers a variety of interesting properties such as: c..
Transformation Temperature, Tg 110 °C
230 °F
10°C/min; ISO 11357-1/-2
EMS-Grivory Grivory® TR 55 LY PA12/MACMI
Product description: Grilamid TR grades are transparent thermoplastic polyamides based on aliphatic and cycloaliphatic blocks. Grilamid TR 55 LY offers a variety of interesting properties such as: c..