Polymer Property : CTE, linear, Parallel to Flow = 98.3 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 177 µm/m-°C

@Temperature 20.0 °C
98.3 µin/in-°F

@Temperature 68.0 °F
Arkema Group Kynar® FLEX 2750 PVDF  (discontinued **)
Designation ISO 12086-VDF/HFP-K, EG1NS, M. ?E7.B.F.A.C,, ? (4-10)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, imperviousne..