CTE, linear, Parallel to Flow 164 µm/m-°C
91.0 µin/in-°F
ASTM D696
Techmer ES HiFill® PA4/6 GF45 HS BK 45% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 45% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackTPCI# 9627150Informat..
CTE, linear, Parallel to Flow 164 µm/m-°C
91.0 µin/in-°F
ASTM D696
Techmer ES HiFill® PA4/6 GF40 HS 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedTPCI# 9627150Information provided by T..