Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 156 µm/m-°C @Temperature 20.0 °C |
86.7 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Lubrizol Estane® 2103-90AEL Film Grade Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product .. |