Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 84.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
47.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP NX10302 PC+ABS (Asia Pacific)
This is a PC/ABS compound with improved plating, surface and mechanical performance, a good candidate for Laser Direct Structuring applications.