Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 82.2 µm/m-°C

@Temperature -40.0 - 100 °C
45.7 µin/in-°F

@Temperature -40.0 - 212 °F
ASTM E831
Proto3000 ABS-M30 Fused Deposition Modeling Polymer
Description: ABS-M30 is up to 25-70 percent stronger than standard Stratasys ABS and is an ideal material for conceptual modeling, functional prototyping, manufacturing tools, and end-use-parts. ABS..
CTE, linear, Parallel to Flow 82.2 µm/m-°C

@Temperature -40.0 - 100 °C
45.7 µin/in-°F

@Temperature -40.0 - 212 °F
ASTM E831
Proto3000 ABS-M30i Fused Deposition Modeling Polymer
Description: ABS-M30i is a high strength material well suited for the medical, pharmaceutical and food packaging industries. Parts manufactured with ABS-M30i material are biocompatible (ISO 10993 ce..