Polymer Property : CTE, linear, Parallel to Flow = 8.40 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 8.40 µm/m-°C

@Temperature 23.0 - 60.0 °C
4.67 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP LCL36E PEEK (Europe-Africa-Middle East)
LNP* LUBRICOMP* LCL36E is a compound based on Polyetheretherketone resin containing Carbon Fiber , PTFE. Added features include : Electrically Conductive, Internally Lubricated, Easy Molding.
CTE, linear, Parallel to Flow 8.40 µm/m-°C

@Temperature 23.0 - 60.0 °C
4.67 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON UEF26AS PPA (Europe-Africa-Middle East)
LNP* Stat-kon* UEF26AS is a compound based on Polyphthalamide resin containing Glass Fiber, Carbon Fiber. Added features of this material include: Electrically Conductive.