Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 143 µm/m-°C @Temperature 23.0 - 60.0 °C |
79.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide P1000IX3 PA6, Impact Modified, Injection Molded Staramide P1000IX3 is an Impact Modified, Polyamide 6 Injection Molding Resin (also known as P1000HI020 or Star X 2020)Information provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 143 µm/m-°C @Temperature 23.0 - 60.0 °C |
79.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermotuf P1000IX3 PA 6 (Europe-Africa-Middle East) LNP* THERMOTUF* P1000IX3 is a compound based on PA6 resin containing Impact Modifier. Added features include : High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |