Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 141 µm/m-°C @Temperature -80.0 - -30.0 °C |
78.3 µin/in-°F @Temperature -112 - -22.0 °F |
ASTM D696 |
Lubrizol Pellethane® 2363-55DE Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |