Polymer Property : CTE, linear, Parallel to Flow = 720 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 720 µm/m-°C

@Temperature -40.0 - 40.0 °C
400 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRILOY ZX06315 PPE+SEBS+Polyolefin (Asia Pacific)
LNP* Lubriloy* ZX06315 is a compound based on PPE+PS Blend resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Internally Lubricated, Non-Brominated & N..
CTE, linear, Parallel to Flow 720 µm/m-°C

@Temperature -40.0 - 40.0 °C
400 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRILOY ZX06315 PPE+SEBS+Polyolefin (Europe-Africa-Middle East)
LNP* Lubriloy* ZX06315 is a compound based on PPE+PS Blend resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Internally Lubricated, Non-Brominated & N..