Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 20.0 °C |
72.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
KEP Kepital® F10 Standard Grade/High Viscosity Acetal Homopolymer Extrusion: electrical parts, machine/mechanical parts, industrial parts, automotive parts, applications, electronic data processing parts, thick-walledKepital® is a registered trademark of Korea .. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 20.0 °C |
72.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
KEP Kepital® F40 Standard Grade/Low Viscosity Acetal Homopolymer injection molding: electrical parts, machine/mechanical parts, industrial parts, automotive applications, electronic data processing.Kepital® is a registered trademark of Korea Engineering Plasti.. |