Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 7.94 µm/m-°C @Temperature -40.0 - 40.0 °C |
4.41 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP QC008 PA6.10 LNP* THERMOCOMP* QC008 is a compound based on Nylon 6/10 containing 40% Carbon Fiber. Added feature of this grade is: Electrically Conductive. |