Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 13.0 µm/m-°C

@Temperature 20.0 °C
7.22 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
DSM Akulon® S223-PG6U (Dry) 33% Glass Reinforced, Impact Modified Nylon 66 (North America)  (discontinued **)&
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
CTE, linear, Parallel to Flow 13.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
7.22 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON DX09315C PC (Asia Pacific)
LNP* Stat-Kon* DX09315C is carbon fiber filled polycarbonate composite with good flow ability, and high level of cleanliness for the most demanding application. A unique feature of this material is ..
CTE, linear, Parallel to Flow 13.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
7.22 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP DF00A1P PC (Asia Pacific)
LNP* Thermocomp* DF00AIP is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High Modulus, low warpage, Non-Brominated & Non..
CTE, linear, Parallel to Flow 13.0 µm/m-°C
7.22 µin/in-°F
ASTM E831
Sumitomo Bakelite North America RX® 643 Fiberglass Reinforced Phenolic
RXÂ 643 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-10.Information pro..
CTE, linear, Parallel to Flow 13.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
7.22 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP JCL36E PES
LNP* LUBRICOMP* JCL36E is a compound based on Polyethersulfone (PES) resin containing 30% Carbon Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant.
CTE, linear, Parallel to Flow 13.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
7.22 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP WCL36 PBT
LNP* LUBRICOMP* WCL36 is a compound based on PBT resin containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Electrically Conductive, Wear Resistant.
CTE, linear, Parallel to Flow 13.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
7.22 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp OC004 PPS - Linear (Europe-Africa-Middle East)
LNP* THERMOCOMP* OC004 is a compound based on PPS-Linear resin containing Carbon Fiber. Added features include : Electrically Conductive.This data was supplied by SABIC-IP for the Europe-Africa-Midd..
CTE, linear, Parallel to Flow 13.0 µm/m-°C
7.22 µin/in-°F
ASTM E831
Sumitomo Bakelite North America XB-22 Fiberglass Reinforced Phenolic Novolac
XB-22 is a fiberglass reinforced phenolic novolac molding compound, with excellent dimensional stability and good strength at elevated temperatures. This material is formulated for low thermal condu..
CTE, linear, Parallel to Flow 13.0 µm/m-°C
7.22 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® TSG-60/4 W PA666-GF60
Product description: Grilon TSG-60/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 60% glass fibers, modified for parts with high thermal demands. Grilon TSG-..
CTE, linear, Parallel to Flow 13.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
7.22 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Starglas OC004 PPS, 20% Carbon Filled, Injection Molded
Starglas OC004 is a 20% Carbon Fiber Reinforced PPS Injection Molding ResinInformation provided by Eurostar.
CTE, linear, Parallel to Flow 13.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
7.22 µin/in-°F

@Temperature 73.4 - 131 °F
DIN 53752
BASF Ultraform® N2650 Z4 (LEV) POM
Description: Is a POM + PUR, elastomer-modified injection-molding grades with high impact strength for clips, snap and fastening elements, also for components subject to impact stress.Information pr..
CTE, linear, Parallel to Flow 13.0 - 16.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
7.22 - 8.89 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 53752
BASF Ultradur B 4500 PBT
Ultradur B4500 is a general-purpose injection molding grade for high-precision, high-toughness, and dimensionally stable engineering parts. It conforms to FDA requirements of 21 CFR 177.1660.
CTE, linear, Parallel to Flow 13.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
7.22 µin/in-°F

@Temperature 73.4 - 131 °F
DIN 53752
BASF Ultraform® N2650 Z2 (LEV) POM
Description: Is a POM + PUR, elastomer-modified injection-molding grades with high impact strength for clips, snap and fastening elements, also for components subject to impact stress.Information pr..
CTE, linear, Parallel to Flow 13.0 - 16.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
7.22 - 8.89 µin/in-°F

@Temperature 73.4 - 176 °F
BASF Ultradur B 4520 PBT
Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade.
CTE, linear, Parallel to Flow 13.0 - 16.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
7.22 - 8.89 µin/in-°F

@Temperature 73.4 - 176 °F
BASF Ultradur B 6550 PBT
Ultradur B 6550 is a high viscosity PBT extrusion grade.Applications; Used for loose buffer tubes for optical fibers, semi-finished products fro machining, profiles and pipes.
CTE, linear, Parallel to Flow 13.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
7.22 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOTUF OF008I PPS - Linear (Europe-Africa-Middle East)
LNP* Thermotuf* OF008I is a compound based on PPS - Linear resin containing Glass Fiber. Added features of this material include: High Impact.