Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 61.7 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® CY2000 PC+ABS Cycoloy resin CY2000 is a flame retardant (FR) PC/ABS blend free from halogen containing FR agents. It was designed to meet CA133 application requirements.This data was supplied by SABIC-IP for the .. |