CTE, linear, Parallel to Flow 58.5 µm/m-°C

@Temperature -30.0 - 30.0 °C
32.5 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP PH0240A PA 6
LNP* THERMOCOMP* PH0240A is a compound based on Nylon 6 resin. Added features of this grade include: High Impact, High Specific Gravity.