Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 103 µm/m-°C @Temperature 20.0 °C |
57.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Texin® 950U Urethane Thermoplastic Elastomer Key Features:UnfilledU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingProfile extrusionSheet extrusionInformation provided by Bayer Polymers.As of 1 September 2015, B.. |
|||
CTE, linear, Parallel to Flow | 103 µm/m-°C @Temperature 20.0 °C |
57.2 µin/in-°F @Temperature 68.0 °F |
ASTM E381 |
Solvay Specialty Polymers Mindel® S-1000 Modified Polysulfone
(discontinued **) This product line was acquired by Solvay Advanced Polymers from BP Amoco in November 2001. |
|||
CTE, linear, Parallel to Flow | 103 µm/m-°C @Temperature 23.0 - 80.0 °C |
57.2 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® CL101D PBT+PC (Europe-Africa-Middle East) XENOY CL101D is an impact modified PBT+PC injection moulding resin with excellent low temperature impact performance. Applications: automotive exterior components such as bumper systems.This data wa.. |