Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 52.8 µm/m-°C @Temperature -30.0 - 30.0 °C |
29.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP NF001 PC+ABS LNP THERMOCOMP* NF001 is a compound based on PC+ABS resin containing 5% Glass Fiber. |