Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 9.60 µm/m-°C | 5.33 µin/in-°F | TMA |
Vyncolit Neopreg Kinel® SK61 L5G Glass Fiber Reinforced Molding Compound Epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particular suited for over molding.. |
|||
CTE, linear, Parallel to Flow | 9.60 µm/m-°C | 5.33 µin/in-°F | TMA |
Vyncolit Neopreg Kinel® SK80 L8G Glass Fiber Reinforced Molding Compound Epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited for over mold.. |