Polymer Property : CTE, linear, Parallel to Flow = 45.5 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 45.5 µm/m-°C

@Temperature -30.0 - 30.0 °C
25.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP DF002 PC
LNP THERMOCOMP* DF002 is a compound based on Polycarbonate resin containing 10% Glass Fiber.
CTE, linear, Parallel to Flow 45.5 µm/m-°C

@Temperature -30.0 - 30.0 °C
25.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP DF002H PC
LNP THERMOCOMP* DF002H is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added feature includes: Healthcare.