Polymer Property : CTE, linear, Parallel to Flow = 40.5 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 40.5 µm/m-°C

@Temperature 40.0 - 120 °C
22.5 µin/in-°F

@Temperature 104 - 248 °F
ASTM E 831
SABIC Innovative Plastics LNP KONDUIT PX11313 PA 6 (Asia Pacific)
Thermally conductive mineral filled PA6 FR compounding
CTE, linear, Parallel to Flow 40.5 µm/m-°C

@Temperature 40.0 - 120 °C
22.5 µin/in-°F

@Temperature 104 - 248 °F
ASTM E 831
SABIC Innovative Plastics LNP KONDUIT PX11313 PA 6 (Europe-Africa-Middle East)
Thermally conductive mineral and glass fiber filled PA6, FR, compliant with ECO protocols, non-brominated, non-chlorinated