Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 38.1 µm/m-°C @Temperature -30.0 - 30.0 °C |
21.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RX96592 PA 66 LNP* Thermocomp* RX96592 is a compound based on Nylon 6/6 containing Proprietary Fillers. |