Polymer Property : CTE, linear, Parallel to Flow = 34.9 µm/m-°C
Polymer Property :
CTE, linear, Parallel to Flow =
34.9 µm/m-°C
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
34.9
µm/m-°C
19.4
µin/in-°F
dry; ISO 11359-1/-2
DSM Akulon® Ultraflow K-FHGM35 PA6-(GF+MD)40
15% Glass Reinforced, Heat Stabilized, High Flow