Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 29.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
16.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOTUF VFK33S PA 66
LNP THERMOTUF* VFK33S is a compound based on Nylon resin containing Glass Fiber, Mineral. Added features of this material include: Heat Stabilized.