Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Parallel to Flow = 2.80 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 2.80 µm/m-°C

@Temperature -40.0 - 40.0 °C
1.56 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON 9X06519 Cyclic Olefinic Copolymer
LNP STAT-KON* 9X06519 is a compound based on Cyclic Olefinic Copolymer resin containing 30% Carbon Fiber. Added features of this material include: Clean Compounding System, Electrically Conductive...
CTE, linear, Parallel to Flow 2.80 µm/m-°C

@Temperature -40.0 - 40.0 °C
1.56 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON 9X06519 Cyclic Olefinic Copolymer (Asia Pacific)
LNP STAT-KON* 9X06519 is a compound based on Cyclic Olefinic Copolymer resin containing Carbon Fiber. Added features of this material include: Clean Compounding System.
CTE, linear, Parallel to Flow 2.80 - 3.40 µm/m-°C

@Temperature 23.0 - 80.0 °C
1.56 - 1.89 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 53752
BASF Ultradur B 4406 G4 PBT
Description: Is a PBT, flame-retardant injection-molding grades, with 20% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh..