Polymer Property : CTE, linear, Parallel to Flow = 195 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 195 µm/m-°C

@Temperature 20.0 °C
108 µin/in-°F

@Temperature 68.0 °F
Arkema Group Pebax® 4033 SN 01 Polyether Block Amide (PEBA) (Conditioned)
POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness..