Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 185 µm/m-°C | 103 µin/in-°F | ISO 11359-1/-2 |
DSM Arnitel® EM631 TPC-ET Extrusion Grade |
|||
CTE, linear, Parallel to Flow | 185 µm/m-°C @Temperature 20.0 °C |
103 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 3200 H Polypropylene Blow moldings and thermoformed parts.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 185 µm/m-°C @Temperature 20.0 °C |
103 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 3200 MC Polypropylene Cast film without slip and blocking agents.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 185 µm/m-°C @Temperature 20.0 °C |
103 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 3225 MC Polypropylene Grade containing slip and blocking agents, for cast film with medium slip.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 185 µm/m-°C @Temperature 20.0 °C |
103 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 3236 MC Polypropylene Grade containing slip, blocking and antistatic agents, for cast film with medium slip.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 185 µm/m-°C @Temperature 20.0 °C |
103 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 3240 NC Polypropylene Grade containing nucleating agent for transparent injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 185 µm/m-°C @Temperature 20.0 °C |
103 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 3248 TC Polypropylene Easy-flowing grade containing nucleating and antistatic agents for transparent injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 185 µm/m-°C @Temperature 20.0 °C |
103 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 3325 MC Polypropylene Grade containing slip and blocking agents, for cast film.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 185 µm/m-°C @Temperature 20.0 °C |
103 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 3336 MC Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 185 µm/m-°C @Temperature 20.0 °C |
103 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 3340 PC Polypropylene Nucleated grade for injection moldings with higher transparency.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 185 µm/m-°C @Temperature 20.0 °C |
103 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 3520 L Polypropylene Grade containing antiblocking agent; sealing layer for OPP film.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 185 µm/m-°C @Temperature 20.0 °C |
103 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 3248 RC Polypropylene Grade containing nucleating and antistatic agents for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 185 µm/m-°C @Temperature 20.0 °C |
103 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 3300 MC Polypropylene Data was collected by ISO methods and provided by BASF. |