Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 179 µm/m-°C | 99.4 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Hytrel® HTR8341G BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Slightly Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers |