Polymer Property : CTE, linear, Parallel to Flow = 160 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 130 - 160 µm/m-°C

@Temperature 23.0 - 80.0 °C
72.2 - 88.9 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
BASF Ultradur® B 4560 PBT
Description: Medium viscosity injection molding grade for industrial parts in the automotive field, for example for head lamp bezel. Suitable for direct metalizing.Information provided by BASF