Polymer Property : CTE, linear, Parallel to Flow = 144 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 144 µm/m-°C
80.0 µin/in-°F
ASTM D696
Techmer ES HiFill® HDPE 8904 UV GY
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV ResistanceAppearance: GreyInformation provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 144 µm/m-°C
80.0 µin/in-°F
ASTM D696
Techmer ES HiFill® HDPE UV
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV ResistanceProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 144 µm/m-°C

@Temperature 23.0 - 60.0 °C
80.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-LOY KX09024 ACETAL COPOLYMER (Europe-Africa-Middle East)
LNP* Statloy* KX09024 is a compound based on Polyacetal with reduced Resistivity. Added features include: Antistatic Properties
CTE, linear, Parallel to Flow 144 µm/m-°C
80.0 µin/in-°F
ASTM D696
Techmer ES HiFill® HDPE
Availability: North AmericaForms: PelletsProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 144 µm/m-°C
80.0 µin/in-°F
ASTM D696
Techmer ES Luriblend® HDPE GL5
Availability: North AmericaForms: PelletsAdditive: Graphite Powder LubricantInformation provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 144 µm/m-°C

@Temperature 23.0 - 60.0 °C
80.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP FP003 PE (Europe-Africa-Middle East)
LNP *Lubricomp* FP003 is a compound based on Polyethylene resin, containing PTFE and Silicone. Added features include: Internally Lubricated.