Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 250 µm/m-°C | 139 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® 2D 25 W 20 HL X black 9992 PA612-I Product Description: Grilamid 2D 25 W 20 HL X black 9992 is a semi-flexible high viscosity, plasticized, high impact and highly heat resistant polyamide 612 (PA612) grade. Unique properties of Gril.. |