Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 138 µm/m-°C | 76.7 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT) Unreinforced Renewably Sourced Polytrimethylene Terephthalate with Excellent Impact Resistance Sorona MT3401 NC010 is a medium toughened polytrimethylene terephthalate resin containing 29% renewably.. |
|||
CTE, linear, Parallel to Flow | 138 µm/m-°C @Temperature 20.0 °C |
76.7 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Rilsan® MB 3501 Nylon 11, Flexible Tubing Grade (Dry) Designation ISO 1874-PA11-HI,MHL,22-004Flexible grade for tubes extrusion. Available color: black. Light and heat stabilized.Flexibility. High burst pressure and impact strength. Fit for use in a wi.. |