Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 124 µm/m-°C @Temperature -30.0 - 30.0 °C |
68.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP TX97446 PU LNP* LUBRICOMP* TX97446 is a compound based on Polyurethane containing Proprietary Fillers. Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 124 µm/m-°C @Temperature 20.0 °C |
68.9 µin/in-°F @Temperature 68.0 °F |
|
Covestro Desmopan® 460 Thermoplastic Polyurethane Desmopan 460 is a TPU on the basis of a special ester.Applications: Bearing shells, gear wheels, seals, cable connectors.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience w.. |