Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 113 µm/m-°C @Temperature 23.0 - 60.0 °C |
62.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP COLORCOMP WX96084 PBT (Europe-Africa-Middle East) LNP* COLORCOMP* WX96084 is a compound based on Polybutylene Terephalate resin. Added features include: Custom Color White. |
|||
CTE, linear, Parallel to Flow | 113 µm/m-°C | 63.0 µin/in-°F | ASTM D696 |
Ravago Manufacturing Americas Hylon® N1000THLUV2 Polyamide 66
(discontinued **) Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Lubricated, Heat Stabilized and Good ToughnessRoHS CompliantAuto Specifications: GM GMP.PA66.079 Color: Bla.. |
|||
CTE, linear, Parallel to Flow | 113 µm/m-°C @Temperature -30.0 - 30.0 °C |
62.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP QP004 PA 6/10 LNP* LUBRICOMP* QP004 is a compound based on Nylon 6/10 containing 20% PTFE/Silicone. Added feature of this grade is: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 113 µm/m-°C @Temperature 23.0 - 60.0 °C |
62.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS (Europe-Africa-Middle East) LNP* Stat-loy* A3000 is a compound based on Acrylonitrile Butadiene Styrene resin. Added features of this material include: Antistat. |
|||
CTE, linear, Parallel to Flow | 113 µm/m-°C @Temperature -30.0 - 30.0 °C |
62.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-LOY AX11421 ABS LNP* STAT-LOY* AX11421 is a compound based on ABS resin. Added feature of this material is: Antistatic. |
|||
CTE, linear, Parallel to Flow | 113 µm/m-°C @Temperature 20.0 °C |
62.8 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Orgalloy® RS 66K15LT Nylon 66 Alloy, Mineral/Impact Grade (Conditioned) RS 66 series, rigid polyamide 66 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional propertie.. |