Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 198 µm/m-°C @Temperature -40.0 - 60.0 °C |
110 µin/in-°F @Temperature -40.0 - 140 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 350U PBT (Asia Pacific) Impact modified, UV stabilised, flame retardant polyester with an internal glowwire rating of 850C on 1.6mm flat plaques.This data was supplied by SABIC-IP for the Asia Pacific region. |