Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 189 µm/m-°C @Temperature 20.0 °C |
105 µin/in-°F @Temperature 68.0 °F |
|
Eastman Ecdel PCCE 9967 Copolyester Ether Elastomer ISO data as provided by the manufacturer, Eastman Chemical |