Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Fusion | 20.0 - 24.0 J/g | 8.60 - 10.3 BTU/lb | Crystallization Heat; ASTM D3417 |
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 21510 PVDF copolymer has low viscosity and is suitable for solution processing in lithium batteries applications.Information provided by Solvay Specialty Polymers. |
|||
Heat of Fusion | 20.0 - 24.0 J/g | 8.60 - 10.3 BTU/lb | ASTM D3417 |
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 21510 PVDF copolymer has low viscosity and is suitable for solution processing in lithium batteries applications.Information provided by Solvay Specialty Polymers. |