Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Fusion | 39.98 J/g | 17.20 BTU/lb | Latent |
Reade Advanced Materials Wood's Metal Alloy (Sn + Pb + Bi + Cd) Description: A low melting fusible alloy.Various granulations are available. Used in heating baths in laboratories, antifriction metals, and solders.Information provided by Reade Advanced Materials.. |